Mixed Deck — All 456A Topics Flashcards
100 cards from real 456A practice questions. Tap to flip, then mark Knew It or Still Learning — missed cards come back until you master them.
Read the first 20 Mixed Deck — All 456A Topics flashcards as text
What is a bird's nest or wire tangle in GMAW, and what causes it?
Answer: A tangle of wire at the drive rolls caused by a blockage in the liner, worn contact tip, excessive drive roll pressure, or wire feeding issues
A bird's nest is a tangled mass of wire that bunches up at the drive rolls. It occurs when the wire cannot feed through the gun — causes include a kinked or clogged liner, worn or wrong-sized contact tip, incorrect drive roll tension, contaminated wire, or a sharp bend in the gun cable. It requires stopping, cutting the tangle, and fixing the root cause.
Which type of oxyfuel flame is characterized by an acetylene feather between the inner cone and outer envelope, and is used for welding high-carbon steel?
Answer: Carburizing (reducing) flame
A carburizing flame has excess acetylene, producing a luminous feather that adds carbon to the weld pool — useful for hard-facing and high-carbon steel applications.
What is 'cold cracking' (hydrogen-induced cracking) in GTAW welds on high-strength low-alloy (HSLA) steel and how is it prevented?
Answer: Cracking that occurs after the weld cools, caused by hydrogen diffusion; prevented by preheat, low-hydrogen filler, clean base metal, and PWHT
Cold cracking (HIC) in GTAW occurs when hydrogen absorbed during welding diffuses to high-stress areas (typically the HAZ) as the weld cools. Prevention includes: preheating to slow cooling and allow hydrogen diffusion, using clean (dry, oxide-free) base metal, minimizing moisture in the shielding gas, and PWHT for thick/restrained joints. GTAW inherently has lower hydrogen than SMAW but is not immune.
What is the recommended included angle for grinding a pointed tungsten tip for DCEN GTAW on steel?
Answer: 2.5× the electrode diameter length, ground longitudinally to produce a consistent tip
For DCEN GTAW, the tungsten should be ground to a point with the length of the taper equal to approximately 2–2.5× the electrode diameter. Grinding should be done longitudinally (along the length of the electrode) to prevent spiral arc deviation. A consistent taper angle concentrates the arc and provides good penetration.
Which type of welding power source characteristic is used for SMAW — constant current (CC) or constant voltage (CV)?
Answer: Constant current (CC)
SMAW uses a constant current (CC) power source, also called a 'drooper.' The output amperage remains relatively constant even if arc length changes, while voltage varies. This characteristic allows the welder to manually control arc length without causing large swings in current.
What is 'weld metal solidification cracking' and which welding parameter most effectively controls it?
Answer: Cracking along weld centreline during solidification; controlled by maintaining a width-to-depth (W/D) ratio greater than 1 and reducing sulfur/phosphorus impurities
Centreline solidification cracking occurs when the last liquid (enriched in impurities like S and P) in the weld pool solidifies under tensile shrinkage stress. A weld bead that is deeper than it is wide (W/D 1 distributes the liquid at the top surface where stresses are lower and prevents centreline crack formation.
Which shielding gas mixture is most commonly used for GMAW on carbon steel in Canada?
Answer: 75% Argon / 25% CO2 (C25)
C25 (75% Ar / 25% CO2) is the most widely used shielding gas for carbon steel GMAW in Canada. It provides a good balance of arc stability, low spatter, good penetration, and bead appearance. Pure CO2 gives deeper penetration but more spatter; pure Ar is used for aluminum and some stainless applications.
What is the Vickers Hardness (HV) limit typically specified for the HAZ in sour service (H2S) environments per NACE MR0175/ISO 15156?
Answer: 250 HV maximum
NACE MR0175/ISO 15156 (materials for sour service) specifies a maximum HAZ hardness of 250 HV (approximately 22 HRC) for carbon and low-alloy steels to prevent sulfide stress cracking (SSC). Harder zones are more susceptible to hydrogen embrittlement from H2S environments. This limit drives preheat, heat input, and PWHT requirements for sour service welding.
What is the recommended method for cleaning aluminum before GTAW welding?
Answer: Degrease with acetone or approved solvent, then remove oxide layer with a stainless steel wire brush dedicated to aluminum
Aluminum cleaning for GTAW requires two steps: first, remove oil and grease with a clean cloth and acetone or approved solvent; second, remove the aluminum oxide layer with a dedicated stainless-steel wire brush (never used on other metals to avoid contamination). The oxide melts at ~2050°C vs. ~660°C for aluminum, so it must be mechanically removed before welding.
What is the minimum lens shade number recommended for SMAW welding at 150–200 amperes, per CSA Z94.3?
Answer: Shade 10
CSA Z94.3 (Eye and Face Protection) recommends a minimum shade 10 filter lens for SMAW welding at 150–200 amperes. Higher amperages require darker shades (up to shade 14) to protect against UV/IR radiation from the arc.
What is 'tungsten inclusion' in GTAW and how is it caused?
Answer: Tungsten particles embedded in the weld metal; caused by the tungsten tip contacting the weld pool or being contaminated
Tungsten inclusion occurs when a piece of the tungsten electrode breaks off and becomes embedded in the weld metal. It is caused by: touching the tungsten to the weld pool, excessive current melting the tip, contamination of the tungsten by the base metal, or improper arc starting technique. Tungsten inclusions are rejectable defects and are highly visible on radiographic film.
What is the purpose of a 'backing bar' in groove weld joint preparation?
Answer: Supports the root pass from the back side, preventing burn-through, ensuring complete root penetration, and allowing single-sided welding where back access is impossible
A backing bar (steel strip for structural work, ceramic or copper for temporary use) is placed behind the root opening. It supports the molten weld pool during the root pass, prevents burn-through, and ensures complete fusion at the root even with a larger root opening (typically 6 mm for backing-bar joints). Steel backing is usually permanently fused into the joint; temporary backings are removed after the root pass.
What is the purpose of a 'weld run-off tab' at the end of a weld joint?
Answer: Allows the weld to be started and terminated on temporary extensions, keeping weld defects (craters, start porosity) off the base metal joint
Run-off tabs (extension bars) are temporary pieces of matching base material tack-welded to the ends of the joint. The weld starts on the run-on tab, proceeds through the joint, and ends on the run-off tab, keeping arc starts and stops (which are prone to porosity, craters, and inclusion) off the structural weld. Tabs are removed and the base metal ends dressed flush after welding.
What is the primary safety hazard associated with SMAW welding in a confined space according to Canadian OHS regulations?
Answer: Oxygen deficiency or accumulation of toxic fumes without adequate ventilation
In a confined space, SMAW produces fumes and gases (including CO, NOx, ozone, and metal fumes) that can displace oxygen or accumulate to toxic levels. Canadian OHS regulations (federal COHSR and provincial equivalents) require atmospheric testing, continuous ventilation, and standby rescue procedures for confined space welding.
What is a GTAW walking the cup technique used for?
Answer: Rocking the ceramic gas cup alternately on each side of the joint to maintain consistent travel speed, torch angle, and arc length while welding pipe or tubing
Walking the cup is a GTAW pipe welding technique where the welder rocks the ceramic gas cup from side to side on the pipe bevel, alternating contact points like walking. This provides consistent torch angle, travel speed, and arc length, producing uniform weave beads — particularly valuable in pipe root and fill passes where consistency is critical.
What is a 'Procedure Qualification Record' (PQR) and how does it relate to a WPS under CSA W47.1?
Answer: A PQR documents the actual parameters used and test results from a qualification test weld; it is the technical basis for writing a WPS
A PQR records the actual welding variables used during the qualification test coupon and the results of destructive/non-destructive tests (tensile, bend, impact, hardness, RT/UT). The PQR proves the WPS is capable of producing sound welds meeting code requirements. One or more PQRs support the writing of a WPS under CSA W47.1.
On a structural drawing, a fillet weld symbol shows '8' to the left and '150-300' to the right of the fillet symbol. What does this specify?
Answer: 8 mm leg fillet welds, 150 mm long, spaced 300 mm apart (intermittent welds)
In standard weld symbol notation: the number to the left of the symbol is the weld size (8 mm leg), and the number(s) to the right indicate weld length and pitch. '150-300' means weld segments 150 mm long at 300 mm pitch (centre-to-centre spacing). This is an intermittent fillet weld specification — commonly used for non-critical connections to reduce heat input and cost.
What is the acceptance criterion for undercut in structural welds under CSA W59 for statically loaded structures?
Answer: Undercut depth not exceeding 1 mm (1/32 in.) for welds transverse to the primary stress direction; 2 mm for welds parallel to the primary stress
CSA W59 (following AWS D1.1) allows limited undercut in statically loaded structures: up to 1 mm depth for welds transverse to tensile stress and up to 2 mm for welds parallel to stress (where the notch is less critical). For dynamically loaded structures (Category C), undercut is more tightly limited. Undercut exceeding limits must be repaired by grinding to a smooth transition or by depositing additional weld metal.
What does a fillet weld symbol look like on a welding drawing?
Answer: A right triangle placed on the reference line with the vertical leg always on the left
The fillet weld symbol is a right triangle with the perpendicular (vertical) leg always on the left side, regardless of the weld orientation. The leg size is written to the left of the symbol. This is the most commonly used welding symbol in structural and general fabrication.
What is the 'P-number' system used for in welding procedure qualification under ASME/CSA standards?
Answer: Groups base metals with similar weldability and metallurgical characteristics to reduce the number of procedure qualifications required
P-numbers group base materials by chemical composition and mechanical properties for qualification purposes. Qualifying a procedure with one material in a P-number group typically qualifies it for welding all materials within that group, reducing the total number of qualification tests. Carbon steels are P1, low-alloy steels are P3-P5, austenitic stainless steels are P8, etc.
How this page was made: written with AI tools and published by Nathan Beja, founder of Practice Test Geeks, who is responsible for its content. Exam facts are checked against the official sources listed below. Not reviewed by a subject-matter expert. Editorial policy
Sources & references
Exam facts on this page (fees, format, dates, passing scores) are checked against these official sources; the date is our last check. Editorial policy
- red-seal.ca — Exam format, exam information · verified Nov 2026
- skilledtradesontario.ca — Passing score, score release, time limit, renewal, score validity, eligibility, retake fee, test delivery, fees, retake policy · verified Nov 2026