← All 456A Flashcard Decks

SMAW (Shielded Metal Arc Welding) Flashcards

6 cards from real 456A practice questions. Tap to flip, then mark Knew It or Still Learning — missed cards come back until you master them.

Read the first 6 SMAW (Shielded Metal Arc Welding) flashcards as text
  1. What does the 'E' in an electrode classification such as E7018 stand for?

    Answer: Electrode

    In the AWS/CSA electrode classification system, 'E' stands for electrode, indicating it is a consumable electrode used in the SMAW process.

  2. In the electrode classification E7018, what does the '70' indicate?

    Answer: Minimum tensile strength of 70,000 psi (480 MPa)

    The first two digits (70) in E7018 represent the minimum tensile strength of the deposited weld metal, which is 70,000 psi or approximately 480 MPa.

  3. What type of current is typically recommended for E7018 low-hydrogen electrodes?

    Answer: DCEP (Direct Current Electrode Positive)

    E7018 low-hydrogen electrodes are recommended for use with DCEP (reverse polarity), which provides deeper penetration and better arc stability. Some formulations also work on AC.

  4. What is the maximum moisture content allowed for low-hydrogen electrodes (E7018) before they must be re-dried according to CSA W48?

    Answer: They must be stored at 120–150°C and used within 4 hours of removal from oven

    CSA W48 requires low-hydrogen electrodes to be stored in ovens at 120–150°C and used within a specified time (typically 4 hours) after removal to prevent hydrogen pickup, which can cause hydrogen-induced cracking.

  5. Which SMAW electrode would be best suited for welding in all positions including overhead?

    Answer: E6013

    E6013 is an all-position electrode with a rutile coating that provides good arc control and slag removal, making it suitable for overhead and vertical welding. E7024, E6020, and E7028 are flat/horizontal position electrodes only.

  6. What is the primary cause of porosity in SMAW welds?

    Answer: Contamination of the weld pool by gas (moisture, oil, or coating breakdown)

    Porosity in SMAW is primarily caused by gas entrapment in the weld pool. Sources include moisture in the electrode coating, oil or grease on base metal, contaminated shielding gas, or improper electrode storage.

How this page was made: written with AI tools and published by Nathan Beja, founder of Practice Test Geeks, who is responsible for its content. Exam facts are checked against the official sources listed below. Not reviewed by a subject-matter expert. Editorial policy

Sources & references

Exam facts on this page (fees, format, dates, passing scores) are checked against these official sources; the date is our last check. Editorial policy

  1. red-seal.ca — Exam format, exam information · verified Nov 2026
  2. skilledtradesontario.ca — Passing score, score release, time limit, renewal, score validity, eligibility, retake fee, test delivery, fees, retake policy · verified Nov 2026