← All 456A Flashcard Decks

SMAW (Shielded Metal Arc Welding) Flashcards

6 cards from real 456A practice questions. Tap to flip, then mark Knew It or Still Learning — missed cards come back until you master them.

Read the first 6 SMAW (Shielded Metal Arc Welding) flashcards as text
  1. Which electrode classification would be most appropriate for welding A516 Grade 70 pressure vessel steel with SMAW?

    Answer: E7016 or E7018

    E7016 or E7018 low-hydrogen electrodes are the standard choice for pressure vessel steels such as A516 Gr 70 because they provide low hydrogen content (preventing HIC), matching tensile strength (~70 ksi/480 MPa), and good toughness. E6010 can be used for root passes.

  2. What is 'slag inclusion' in a SMAW weld and what is the primary prevention method?

    Answer: Slag trapped in the weld metal; prevented by thorough inter-pass slag removal and proper technique

    Slag inclusion occurs when solidified flux (slag) becomes trapped within the weld metal during multi-pass welding. Prevention includes thorough chipping and wire brushing between passes, maintaining proper electrode angle to keep the slag behind the weld pool, and using adequate amperage.

  3. What does 'burn-through' mean and what is the most likely cause in SMAW on thin material?

    Answer: Complete melting through the base metal; caused by excessive amperage or slow travel speed

    Burn-through is when the arc completely melts through the base metal, creating a hole. On thin material, it is most commonly caused by excessive amperage, too slow a travel speed, or excessive dwell time in one area. Reducing amperage and increasing travel speed are the primary remedies.

  4. In SMAW welding of pipe in the 6G position, what does the '6G' designation mean?

    Answer: Pipe axis at 45° to horizontal, pipe fixed (not rotated)

    The 6G position has the pipe axis fixed at 45° to the horizontal. Because the pipe is not rotated, the welder must weld in all positions (flat, vertical, overhead) in a single joint, making it the most demanding qualification test position.

  5. What is 'overlap' (cold lap) as a weld discontinuity in SMAW?

    Answer: Weld metal that extends beyond the weld toe onto the base metal without fusing to it

    Overlap (cold lap) occurs when molten weld metal rolls over the toe of the weld and solidifies on the base metal without fusing to it. It is caused by too low an amperage, incorrect electrode angle, or too slow a travel speed. It creates a notch effect and is a rejectable defect.

  6. When welding dissimilar metals with SMAW, what is the general rule for electrode selection?

    Answer: Select an electrode that matches or slightly undermatches the lower-strength base metal

    When joining dissimilar strength metals, it is generally recommended to use an electrode that matches or slightly undermatches (undermatch) the weaker of the two base metals. This prevents a brittle transition and allows the joint to deform in the weaker material rather than failing catastrophically at the weld.

How this page was made: written with AI tools and published by Nathan Beja, founder of Practice Test Geeks, who is responsible for its content. Exam facts are checked against the official sources listed below. Not reviewed by a subject-matter expert. Editorial policy

Sources & references

Exam facts on this page (fees, format, dates, passing scores) are checked against these official sources; the date is our last check. Editorial policy

  1. red-seal.ca — Exam format, exam information · verified Nov 2026
  2. skilledtradesontario.ca — Passing score, score release, time limit, renewal, score validity, eligibility, retake fee, test delivery, fees, retake policy · verified Nov 2026