MIG/FCAW (GMAW & Flux-Cored Arc Welding) Flashcards
6 cards from real 456A practice questions. Tap to flip, then mark Knew It or Still Learning — missed cards come back until you master them.
Read the first 6 MIG/FCAW (GMAW & Flux-Cored Arc Welding) flashcards as text
What is 'metal transfer' in GMAW and which mode provides the highest deposition rate?
Answer: The way weld metal moves from the wire to the pool; spray transfer provides the highest deposition rate
Metal transfer describes the mode by which molten metal moves from the electrode wire to the weld pool. Spray transfer (above the transition current) transfers fine droplets axially at high frequency, providing the highest deposition rate and smooth, spatter-free welds. It is limited to flat/horizontal positions due to pool fluidity.
What is the purpose of a push-pull wire feed system in GMAW?
Answer: Maintains consistent wire feed speed over long distances by using drive motors at both the feeder and the gun
In push-pull systems, a motor at the wire feeder pushes the wire through the conduit while a motor in the gun pulls it. This maintains consistent, slip-free feeding over long cable distances (up to 15m) and is especially important for soft wires like aluminum that are prone to birdnesting in push-only systems.
When GMAW welding aluminum with the spray transfer mode, which polarity is required?
Answer: DCEP (Direct Current Electrode Positive)
DCEP is required for GMAW aluminum because the positive electrode polarity provides cathodic cleaning — the arc bombardment breaks up the tenacious aluminum oxide layer on the base metal surface, ensuring good fusion. DCEN does not provide this cleaning action and results in poor weld quality on aluminum.
What is 'birdnesting' in GMAW and what causes it?
Answer: Wire bunching inside the feed system between the drive rolls and contact tip; caused by wire feed obstructions or misaligned components
Birdnesting occurs when wire cannot advance through the liner or contact tip and buckles, creating a tangled mass (resembling a bird's nest) inside the feeder or gun. Causes include a clogged/kinked liner, an oversized contact tip, excessive wire tension, or drive roll misalignment. It requires stopping welding to clear the jam.
What does 'weld profile' refer to and what are the CSA W59 requirements for a fillet weld profile?
Answer: The cross-sectional shape of the weld; should be flat to slightly convex with full fusion to both toes and no undercut exceeding 1 mm
Weld profile describes the cross-sectional shape of a completed weld. CSA W59 requires fillet welds to have flat to slightly convex face profiles, complete fusion to both toes, no undercut exceeding 1 mm for most applications, and no overlap. Excessive convexity creates a stress riser at the toe and wastes weld metal.
What is the significance of the 'A-number' in welding procedure qualification under CSA W47.1/W59?
Answer: It classifies deposited weld metal by chemical composition for procedure qualification purposes
A-numbers classify filler metal deposits by chemical composition (carbon, manganese, silicon, chromium, etc. ranges). Under ASME/CSA qualification rules, the A-number of the filler metal used in a procedure qualification test must match the A-number of the filler metal used in production welding (unless otherwise supported by test data).
How this page was made: written with AI tools and published by Nathan Beja, founder of Practice Test Geeks, who is responsible for its content. Exam facts are checked against the official sources listed below. Not reviewed by a subject-matter expert. Editorial policy
Sources & references
Exam facts on this page (fees, format, dates, passing scores) are checked against these official sources; the date is our last check. Editorial policy
- red-seal.ca — Exam format, exam information · verified Nov 2026
- skilledtradesontario.ca — Passing score, score release, time limit, renewal, score validity, eligibility, retake fee, test delivery, fees, retake policy · verified Nov 2026