← All 456A Flashcard Decks

MIG/FCAW (GMAW & Flux-Cored Arc Welding) Flashcards

6 cards from real 456A practice questions. Tap to flip, then mark Knew It or Still Learning — missed cards come back until you master them.

Read the first 6 MIG/FCAW (GMAW & Flux-Cored Arc Welding) flashcards as text
  1. What is the correct procedure when porosity is found in a GMAW weld due to suspected shielding gas loss?

    Answer: Check gas flow rate, hose connections, and nozzle for blockage; test on scrap before resuming production welding

    When porosity indicates shielding gas issues, the welder must systematically check: flow rate (typically 15–20 L/min for C25), hose connections for leaks, nozzle cleanliness, and draft/wind conditions. Testing on scrap confirms the fix before resuming production welding to avoid rejectable welds.

  2. What is the minimum recommended shielding gas flow rate for GMAW carbon steel welding (C25) to ensure adequate coverage?

    Answer: 15–20 L/min (30–40 CFH)

    A flow rate of 15–20 L/min (approximately 30–40 CFH) is the standard range for GMAW with C25 shielding gas. Too low a flow rate provides inadequate protection; too high a flow rate causes turbulence that can draw in atmospheric air, both resulting in porosity.

  3. What is 'lack of fusion' (LOF) in GMAW and what typically causes it?

    Answer: Weld metal that does not bond to the base metal or previous pass; caused by insufficient heat input or improper technique

    Lack of fusion occurs when the weld metal and base metal (or adjacent weld passes) are in contact but not metallurgically bonded. Causes include too low an amperage/voltage, too fast a travel speed, improper electrode angle directing the arc away from the fusion face, or a dirty/oxidized base metal surface.

  4. When welding with an E71T-1C flux-cored electrode, what does the 'C' suffix indicate?

    Answer: CO2 shielding gas is required

    In the AWS A5.20 (and CSA equivalent) flux-cored electrode classification, the 'C' suffix on FCAW electrodes (e.g., E71T-1C) indicates that pure CO2 shielding gas is required. An 'M' suffix indicates mixed gas (Ar/CO2). Some electrodes are rated for both (C/M).

  5. What is the main advantage of FCAW-G over SMAW for structural welding?

    Answer: Higher deposition rate and continuous wire feed allowing longer welds without stopping to change electrodes

    FCAW-G offers significantly higher deposition rates than SMAW (up to 4–5× faster) and uses continuous wire so the welder does not need to stop to change electrodes. This increases productivity, reduces labour costs, and is why FCAW-G has largely replaced SMAW in structural fabrication shops.

  6. What does the term 'duty cycle' mean for a GMAW power source?

    Answer: The percentage of a 10-minute period that the machine can weld at a rated amperage without overheating

    Duty cycle is expressed as a percentage of a 10-minute interval. A machine rated at 300A at 60% duty cycle can weld at 300A for 6 minutes out of every 10 minutes. Exceeding the duty cycle activates thermal protection (overtemp cutout). Higher duty cycles are needed for production FCAW and GMAW applications.

How this page was made: written with AI tools and published by Nathan Beja, founder of Practice Test Geeks, who is responsible for its content. Exam facts are checked against the official sources listed below. Not reviewed by a subject-matter expert. Editorial policy

Sources & references

Exam facts on this page (fees, format, dates, passing scores) are checked against these official sources; the date is our last check. Editorial policy

  1. red-seal.ca — Exam format, exam information · verified Nov 2026
  2. skilledtradesontario.ca — Passing score, score release, time limit, renewal, score validity, eligibility, retake fee, test delivery, fees, retake policy · verified Nov 2026