What is the difference between FCAW-S (self-shielded) and FCAW-G (gas-shielded) flux-cored welding?
Answer: FCAW-S uses flux in the core to generate its own shielding; FCAW-G requires an external shielding gas in addition to the flux core
FCAW-S electrodes contain flux ingredients that generate all necessary shielding gases and slag without external gas, making them ideal for outdoor/field welding where wind would disperse external shielding. FCAW-G electrodes use a combination of flux core and external shielding gas for better weld quality and lower fume generation.
What is the travel angle and work angle convention for GMAW in the flat position?
Answer: Work angle 90° to the joint; travel angle 5–15° drag (backhand)
For flat position GMAW, the work angle is 90° perpendicular to the joint (or split equally for fillet welds at ~45°), and the travel angle is a 5–15° drag (backhand/trailing) angle pointing back toward the completed weld. This provides good visibility of the weld pool and proper penetration.
What does 'wire stick-out' (contact tip-to-work distance) affect in GMAW?
Answer: Current draw and deposition rate — longer stick-out reduces current and deposition rate
Wire stick-out (the distance from contact tip to workpiece) affects resistance heating of the wire. Longer stick-out increases resistance, preheats the wire, and reduces the actual welding current drawn for the same wire feed speed, lowering penetration and deposition rate. Shorter stick-out increases current and penetration.
What is 'spatter' in GMAW and what is the primary cause when using C25 shielding gas?
Answer: Small droplets of metal expelled from the arc; caused by incorrect voltage/amperage settings or contaminated base metal
Spatter consists of small molten metal droplets expelled from the arc that solidify on the base metal or nozzle. In GMAW with C25, the primary causes are voltage too low or too high relative to wire feed speed, arc instability from contamination, or improper inductance settings. Spatter is non-fused and does not contribute to weld strength.
Which GMAW transfer mode is recommended for welding out-of-position (vertical, overhead)?
Answer: Short-circuit transfer
Short-circuit transfer uses lower heat input and produces a smaller, more controllable weld pool that solidifies quickly, making it suitable for out-of-position welding. Spray transfer produces a large, fluid weld pool that is difficult to control in vertical or overhead positions. Pulse spray can also be used out of position.
What is the purpose of the inductance setting on a GMAW power source?
Answer: Controls the rate of current rise during short circuits, reducing spatter and smoothing bead appearance
Inductance (measured in henries) controls how quickly current rises during the short-circuit phase. Higher inductance slows the current rise, reducing spatter and producing a flatter bead. Lower inductance allows faster current rise for more aggressive penetration but increases spatter. It is typically adjusted for the wire diameter and metal thickness.
How this page was made: written with AI tools and published by Nathan Beja, founder of Practice Test Geeks, who is responsible for its content. Exam facts are checked against the official sources listed below. Not reviewed by a subject-matter expert. Editorial policy
Sources & references
Exam facts on this page (fees, format, dates, passing scores) are checked against these official sources; the date is our last check. Editorial policy
- red-seal.ca — Exam format, exam information · verified Nov 2026
- skilledtradesontario.ca — Passing score, score release, time limit, renewal, score validity, eligibility, retake fee, test delivery, fees, retake policy · verified Nov 2026