← All 456A Flashcard Decks

Metallurgy & Heat Treatment Flashcards

6 cards from real 456A practice questions. Tap to flip, then mark Knew It or Still Learning — missed cards come back until you master them.

Read the first 6 Metallurgy & Heat Treatment flashcards as text
  1. What is the purpose of 'quench and temper' heat treatment for structural steel plates (e.g., A514/T1 steel)?

    Answer: Produces a fine martensitic microstructure with high strength and toughness not achievable by normalizing alone

    Quench and temper (Q&T) heat treatment produces the high-strength, high-toughness microstructure of steels like A514 (T-1). The steel is austenitized, water or oil quenched to form martensite, then tempered to reduce brittleness while maintaining high strength. Q&T steels require special welding procedures to avoid softening the HAZ and must use low-hydrogen processes.

  2. What does 'ferrite number' (FN) indicate in stainless steel weld metal?

    Answer: The amount of delta ferrite in the austenitic weld microstructure; 3–8 FN is typically targeted to prevent hot cracking

    Delta ferrite in austenitic stainless steel weld metal prevents hot (solidification) cracking by interrupting the continuous austenite grain boundaries where low-melting films form. The target FN of 3–8 provides hot crack resistance without excessive ferrite, which can reduce corrosion resistance and toughness. FN is predicted by the Schaeffler or WRC-1992 diagrams from the weld metal composition.

  3. What is the 'critical cooling rate' for a steel?

    Answer: The minimum cooling rate that produces a fully martensitic structure, bypassing pearlite and bainite transformations

    The critical cooling rate is the minimum rate at which austenite must be cooled to suppress all diffusional transformations (pearlite, bainite) and produce a fully martensitic structure. Steels with higher hardenability (higher CE) have lower critical cooling rates and therefore form martensite more easily — including in the HAZ during normal welding cooling conditions.

  4. What is the Ac1 temperature in steel and why is it important for PWHT?

    Answer: The lower critical temperature (~727°C) below which austenite transforms to ferrite+carbide on cooling; PWHT must be performed below this temperature to avoid re-austenitizing the steel

    Ac1 is the temperature at which austenite begins to form during heating (approximately 727°C for carbon steel). PWHT stress relief must be performed below Ac1 to avoid re-austenitizing portions of the HAZ, which would defeat the purpose of the treatment and could introduce new hard zones upon cooling. Typical stress relief temperatures (595–650°C) provide a margin below Ac1.

  5. What is the 'dilution' in weld metal and how does it affect weld metal properties?

    Answer: The percentage of base metal melted into the weld pool; higher dilution shifts weld metal composition toward the base metal composition

    Dilution is the percentage of the weld metal composition contributed by the melted base metal (vs. the filler metal). High dilution means the weld chemistry is heavily influenced by the base metal. In cladding or overlay applications, multiple layers reduce dilution of the top layer. In dissimilar metal welding, dilution affects whether the weld metal composition produces the desired microstructure.

  6. What is the difference between 'yield strength' and 'ultimate tensile strength' (UTS) of a weld metal?

    Answer: Yield strength is the stress at which permanent deformation begins; UTS is the maximum stress the material can withstand before fracture

    Yield strength (0.2% proof stress in Canada, MPa) is the stress at which the material begins to deform plastically (permanently). UTS is the maximum engineering stress reached before the specimen fractures in a tensile test. Weld filler metals are classified by their minimum UTS (e.g., E7018 = 70 ksi/480 MPa UTS minimum). Structural design typically uses yield strength as the allowable stress basis.

How this page was made: written with AI tools and published by Nathan Beja, founder of Practice Test Geeks, who is responsible for its content. Exam facts are checked against the official sources listed below. Not reviewed by a subject-matter expert. Editorial policy

Sources & references

Exam facts on this page (fees, format, dates, passing scores) are checked against these official sources; the date is our last check. Editorial policy

  1. red-seal.ca — Exam format, exam information · verified Nov 2026
  2. skilledtradesontario.ca — Passing score, score release, time limit, renewal, score validity, eligibility, retake fee, test delivery, fees, retake policy · verified Nov 2026