Under AWS D1.1, which weld discontinuity is classified as a 'crack' and is always rejectable regardless of size?
Answer: Any crack regardless of orientation or location in the weld or HAZ
AWS D1.1 classifies cracks as unacceptable discontinuities — cracks of any type, size, or orientation in welds or base metal heat-affected zones are cause for rejection with no minimum size threshold.
What is the purpose of a guided bend test in weld procedure qualification?
Answer: Evaluate the ductility and soundness of the weld and fusion zone by bending specimens around a die of specified radius
The guided bend test bends weld specimens (face, root, or side bends) around a specified radius mandrel/die to assess ductility and reveal discontinuities such as lack of fusion, cracks, and porosity that would open up during bending.
Which ultrasonic testing (UT) technique is most commonly used for weld inspection per AWS D1.1?
Answer: Straight-beam and angle-beam pulse-echo UT using A-scan presentation
AWS D1.1 Annex K specifies conventional pulse-echo UT using straight-beam (0°) and angle-beam (typically 45°, 60°, 70°) transducers with A-scan amplitude presentation as the standard method for weld inspection.
What is the minimum overlap required for radiographic film to ensure full coverage of a weld in AWS D1.1?
Answer: 13 mm (½ in.) minimum overlap between adjacent radiographs
AWS D1.1 requires a minimum of 13 mm (½ in.) overlap between adjacent radiographic exposures to ensure that the entire weld volume is covered with no unexamined gaps.
What is the CWI's responsibility when a WPS lists a heat input range and the welder is found to be significantly exceeding the maximum?
Answer: Stop welding, document the non-conformance, and require the welder to comply with the approved WPS parameters
The CWI must enforce compliance with the approved WPS. Exceeding specified heat input limits is a code violation that can affect weld properties, HAZ microstructure, and qualification basis — welding must stop and non-conformance documented.
In magnetic particle testing (MT), what type of current is most effective for detecting subsurface discontinuities?
Answer: Direct current (DC)
DC and full-wave rectified AC produce a magnetic field that penetrates deeper into the material (up to 6–9 mm subsurface), making them more effective for detecting subsurface discontinuities compared to AC.
Written and edited by Nathan Beja, founder of Practice Test Geeks, with AI assistance. Exam facts are checked against the official sources linked below. Editorial policy
Sources & references
Exam facts on this page (fees, format, dates, passing scores) are checked against these official sources; the date is our last check. Editorial policy
- aws.amazon.com — Fees, exam format, time limit, score validity, renewal, passing score, retake fee, retake policy, score release, test delivery · verified Nov 2026