  1. According to AWS D1.1, what is the minimum preheat temperature required for ASTM A36 steel with a thickness greater than 38 mm (1.5 in.) when using a low-hydrogen process?

    Answer: 107°C (225°F)

    AWS D1.1 Table 4.2 requires a minimum preheat and interpass temperature of 107°C (225°F) for A36 steel greater than 38 mm thick when using a low-hydrogen process.

  2. Which destructive test is specifically used to evaluate the toughness (notch toughness) of weld metal and HAZ?

    Answer: Charpy V-notch impact test

    The Charpy V-notch (CVN) impact test measures the energy absorbed when a notched specimen is fractured by a swinging pendulum, providing a direct measure of material toughness at a specified temperature.

  3. During visual inspection of a completed weld, what measurement tool is used to verify weld size (leg size) of a fillet weld?

    Answer: Fillet weld gauge (weld gauge)

    A fillet weld gauge (such as an AWS fillet weld gauge or bridge cam gauge) is specifically designed to measure the actual leg size of fillet welds quickly and accurately during visual inspection.

  4. Which nondestructive testing (NDT) method is most effective for detecting subsurface discontinuities in austenitic stainless steel welds that cannot be detected by UT due to coarse grain structure?

    Answer: Radiographic testing (RT)

    Radiographic testing (RT) uses X-rays or gamma rays that penetrate the weld regardless of grain structure, making it effective for detecting internal voids, porosity, and inclusions in austenitic stainless steel where UT may be unreliable.

  5. What does the term 'interpass temperature' mean in welding inspection?

    Answer: The maximum temperature of the weld deposit and surrounding base metal between passes in a multi-pass weld

    Interpass temperature is the temperature of the weld joint area (weld deposit and adjacent base metal) at the time of welding just before each subsequent pass is started in a multi-pass weld.

  6. In liquid penetrant testing (PT), what is the purpose of the developer?

    Answer: Draw the penetrant out of discontinuities and provide a contrasting background to enhance defect visibility

    The developer draws (blots) the penetrant that has been trapped in surface-open discontinuities back to the surface by capillary action and absorption, spreading it to create a visible indication against the white developer background.

Written and edited by , founder of Practice Test Geeks, with AI assistance. Exam facts are checked against the official sources linked below. Editorial policy

Sources & references

Exam facts on this page (fees, format, dates, passing scores) are checked against these official sources; the date is our last check. Editorial policy

  1. aws.amazon.com — Fees, exam format, time limit, score validity, renewal, passing score, retake fee, retake policy, score release, test delivery · verified Nov 2026
Welding Inspection & Testing Flashcards — AWS Study Cards with Answers