  1. Which NDE method is best suited for detecting surface and near-surface cracks in ferromagnetic welds?

    Answer: Magnetic particle testing (MT)

    Magnetic particle testing (MT) is the most sensitive and practical method for detecting surface and near-surface (up to ~1/4 inch) cracks in ferromagnetic materials like carbon and low-alloy steel welds.

  2. Liquid penetrant testing (PT) is applicable to:

    Answer: Any material — ferromagnetic and non-ferromagnetic alike

    Liquid penetrant testing works on any non-porous material regardless of magnetic properties — it detects surface-open discontinuities in metals, ceramics, and plastics alike.

  3. Lack of fusion (LOF) in a groove weld is best detected by:

    Answer: Ultrasonic testing (UT)

    Ultrasonic testing (UT) is most effective for detecting lack of fusion because planar defects (LOF, cracks) perpendicular to the ultrasonic beam reflect strong signals, while RT often misses planar defects oriented parallel to the X-ray beam.

  4. Lamellar tearing in welded joints occurs:

    Answer: In the base metal below the HAZ in low-ductility, through-thickness directions of rolled plate

    Lamellar tearing occurs in the base metal below and parallel to the fusion line in rolled plate with low through-thickness ductility, caused by through-thickness contraction stresses during weld cooling.

  5. What does 'Charpy V-notch' (CVN) impact testing measure in weld procedure qualification?

    Answer: The fracture toughness (energy absorbed during fracture) at specified temperatures

    CVN testing measures the energy (in ft-lbs or Joules) absorbed by a notched specimen during fracture impact, characterizing the weld metal's fracture toughness and ductile-to-brittle transition temperature.

  6. A weld that fails the guided bend test during procedure qualification typically indicates:

    Answer: Lack of fusion, excessive porosity, or cracking in the weld joint

    Guided bend test failures indicate insufficient ductility in the weld joint, usually caused by lack of fusion, cracks, excessive porosity, or slag inclusions that open up under the bending deformation.

Written and edited by , founder of Practice Test Geeks, with AI assistance. Exam facts are checked against the official sources linked below. Editorial policy

Sources & references

Exam facts on this page (fees, format, dates, passing scores) are checked against these official sources; the date is our last check. Editorial policy

  1. aws.amazon.com — Fees, exam format, time limit, score validity, renewal, passing score, retake fee, retake policy, score release, test delivery · verified Nov 2026