← All AWS Flashcard Decks

Welding Defects & Quality Control Flashcards

6 cards from real AWS practice questions. Tap to flip, then mark Knew It or Still Learning — missed cards come back until you master them.

Read the first 6 Welding Defects & Quality Control flashcards as text
  1. A welder's continuity of qualification under AWS D1.1 is maintained when:

    Answer: The welder has welded with the qualified process at least once in the preceding 6 months

    AWS D1.1 Clause 4.15 requires welders to use the qualified process at least once in each 6-month period to maintain qualification; absence longer than 6 months requires re-qualification.

  2. Which destructive test is used during procedure qualification under AWS D1.1 to evaluate weld soundness and ductility?

    Answer: Guided bend test

    The guided bend test (both face and root bend) is the standard destructive test for AWS D1.1 procedure qualification, evaluating weld soundness by bending specimens around a mandrel to reveal discontinuities.

  3. Hydrogen-induced cracking (HIC) in welded joints is characterized by its:

    Answer: Delayed onset — cracks can appear hours to days after welding, after the weld has cooled

    HIC (also called delayed or cold cracking) occurs after the weld cools, often appearing hours to days later, because hydrogen diffusion and stress buildup take time after welding to initiate cracks.

  4. The purpose of post-weld heat treatment (PWHT) on carbon steel weldments is primarily to:

    Answer: Reduce residual stresses, temper hard HAZ microstructure, and allow hydrogen to diffuse out

    PWHT (stress relief heat treatment) at 1050–1250°F reduces weld residual stresses, tempers hard martensite/bainite in the HAZ to improve toughness and ductility, and promotes hydrogen diffusion out of the weld zone.

  5. When a CWI (Certified Welding Inspector) performs in-process inspection under AWS D1.1, they must verify:

    Answer: Preheat compliance, inter-pass temperature, electrode type, WPS adherence, and pass-by-pass visual quality

    In-process inspection by a CWI includes continuous verification: preheat and interpass temperatures, electrode type and storage (low-H), WPS compliance (amperage, voltage, travel speed, position), and visual inspection of each weld pass before the next is deposited.

  6. Macro-etch testing of a fillet weld in procedure or welder qualification testing verifies:

    Answer: The actual weld size, throat dimension, fusion, and internal soundness through cross-sectional examination

    Macro-etch testing cuts and etches a cross-section through the fillet weld, revealing the actual leg size, throat, fusion zone shape, root penetration, and any internal discontinuities such as porosity, cracks, or lack of fusion.

Written and edited by , founder of Practice Test Geeks, with AI assistance. Exam facts are checked against the official sources linked below. Editorial policy

Sources & references

Exam facts on this page (fees, format, dates, passing scores) are checked against these official sources; the date is our last check. Editorial policy

  1. aws.amazon.com — Fees, exam format, time limit, score validity, renewal, passing score, retake fee, retake policy, score release, test delivery · verified Nov 2026