← All AWS Flashcard Decks

Welding Defects & Quality Control Flashcards

6 cards from real AWS practice questions. Tap to flip, then mark Knew It or Still Learning — missed cards come back until you master them.

Read the first 6 Welding Defects & Quality Control flashcards as text
  1. A weld with excessive convexity (high crown) is problematic because:

    Answer: It creates stress concentration at the weld toes and may indicate improper deposition technique

    Excessive weld convexity creates a sharp geometric notch at the weld toes (junction between weld face and base metal), which concentrates stress and significantly reduces fatigue life under cyclic loading.

  2. Incomplete joint penetration (IJP) in a groove weld is distinguished from incomplete fusion by:

    Answer: IJP is failure to achieve the specified joint penetration depth at the root; incomplete fusion is lack of bonding between weld and base metal at any location

    IJP specifically refers to inadequate penetration depth at the root of the joint (root pass doesn't reach the specified root depth), while incomplete fusion refers to any lack of bonding between weld metal and base metal at any interface in the joint.

  3. The Brinell Hardness Number (BHN) for typical E7018 deposited weld metal is approximately:

    Answer: 150–200 BHN (typical for as-deposited carbon steel weld metal)

    As-deposited E7018 weld metal typically has a hardness in the 150–200 BHN range, compatible with the 70 ksi yield strength and ductile properties it is designed to provide.

  4. During radiographic testing (RT) of a weld, the image quality indicator (IQI) or penetrameter is used to:

    Answer: Verify that the radiographic technique has sufficient sensitivity to detect minimum rejectable discontinuities

    The IQI (penetrameter) verifies that the RT technique has adequate sensitivity — that discontinuities at or above the minimum rejectable size would be detectable on that specific radiograph.

  5. Weld distortion (angular and longitudinal) is best controlled during fabrication by:

    Answer: Pre-setting (presetting parts in opposite direction of expected distortion), balanced welding, and minimizing weld volume

    Pre-setting parts against expected distortion, using balanced welding sequences (both sides of joint, backstep), and minimizing weld metal volume through proper joint design are the most effective distortion control methods.

  6. Under ASME Section IX, an essential variable for welder performance qualification is defined as:

    Answer: A variable whose change requires re-qualification of the welder

    An essential variable in ASME Section IX is a variable whose change requires the welder to be re-tested and re-qualified — its change significantly affects the ability of the welder to deposit sound welds.

Written and edited by , founder of Practice Test Geeks, with AI assistance. Exam facts are checked against the official sources linked below. Editorial policy

Sources & references

Exam facts on this page (fees, format, dates, passing scores) are checked against these official sources; the date is our last check. Editorial policy

  1. aws.amazon.com — Fees, exam format, time limit, score validity, renewal, passing score, retake fee, retake policy, score release, test delivery · verified Nov 2026