← All AWS Flashcard Decks

Shielded Metal Arc Welding (SMAW) Flashcards

6 cards from real AWS practice questions. Tap to flip, then mark Knew It or Still Learning — missed cards come back until you master them.

Read the first 6 Shielded Metal Arc Welding (SMAW) flashcards as text
  1. The E6013 electrode is preferred for beginners and sheet metal because:

    Answer: It has a soft arc, easy slag removal, and tolerance for poor fit-up — ideal for thinner materials

    E6013 uses a titania-potassium coating that produces a soft, forgiving arc, easily removed slag, and shallow penetration — well-suited for sheet metal, maintenance welding, and beginners.

  2. Which measurement is used to select the correct SMAW electrode diameter?

    Answer: The base metal thickness (thicker metal = larger diameter electrode)

    Electrode diameter is primarily selected based on base metal thickness — thicker material requires larger diameter electrodes that can carry higher currents for adequate penetration and deposition.

  3. Crater cracking in SMAW most commonly occurs:

    Answer: At the end of the weld bead where the crater is not properly filled

    Crater cracks form at the end of a weld bead in the unfilled depression (crater) left when the arc is extinguished; the crater is the last metal to solidify and is susceptible to centerline solidification cracks.

  4. What is the maximum amperage range for an E6010 3/32-inch diameter electrode?

    Answer: 40–80 amperes

    A 3/32-inch E6010 electrode is typically used at 40–80 amperes, with 60–80 being common for most applications. Exact ranges vary by manufacturer.

  5. Stringer beads in SMAW are preferred over weave beads in low-hydrogen applications because:

    Answer: Stringer beads limit heat input per pass, reducing HAZ width, improving toughness, and meeting hydrogen management requirements

    Stringer beads limit heat input per pass, resulting in narrower HAZ, faster cooling, and better mechanical properties (especially toughness and tensile strength) than wide weave beads.

  6. An SMAW welder encounters severe porosity while welding outdoors in cold weather. The most likely cause is:

    Answer: Moisture condensation on the cold base metal contaminating the arc atmosphere

    Cold base metal promotes moisture condensation — water on the surface decomposes in the arc, releasing hydrogen and oxygen that cause porosity. Preheat eliminates this condensation.

Written and edited by , founder of Practice Test Geeks, with AI assistance. Exam facts are checked against the official sources linked below. Editorial policy

Sources & references

Exam facts on this page (fees, format, dates, passing scores) are checked against these official sources; the date is our last check. Editorial policy

  1. aws.amazon.com — Fees, exam format, time limit, score validity, renewal, passing score, retake fee, retake policy, score release, test delivery · verified Nov 2026