The AWS classification E7018 indicates which electrode properties?
Answer: 70 ksi tensile, all-position, AC/DCEP, low-hydrogen potassium
E7018: E=electrode, 70=70 ksi tensile, 1=all-position, 8=low-hydrogen potassium coating, usable with AC or DCEP.
Why must E7018 electrodes be stored in a rod oven?
Answer: To prevent moisture absorption by the low-hydrogen coating, which causes hydrogen-induced cracking
Low-hydrogen coatings are hygroscopic — they absorb moisture from the air. Moisture releases hydrogen into the weld, causing hydrogen-induced cracking (HIC). Storage in rod ovens (250–350°F) keeps the coating dry.
When welding in the overhead (4G/4F) position with SMAW, what technique adjustment is most important?
Answer: Reducing amperage and using a shorter arc length to control the molten pool
In overhead position, reducing amperage and maintaining a short arc length produces a smaller, more controllable weld pool that resists falling from gravity.
Which SMAW electrode coating type is best suited for pipeline root passes because of its deep penetration and suitability for vertical-down welding?
Answer: E6010 (cellulosic, high-cellulose sodium)
E6010 uses a high-cellulose sodium coating that produces a forceful, deeply penetrating arc ideal for open-root joint welding in all positions including vertical down (5G pipeline technique).
Arc blow in SMAW DC welding is caused by:
Answer: Magnetic fields around the base metal deflecting the arc
Arc blow is the deflection of the welding arc by magnetic forces created by the interaction of the DC welding current with the magnetic fields in the base metal, fixtures, or earth ground connections.
Undercut in SMAW is most commonly caused by:
Answer: Too high amperage, too fast travel speed, or incorrect electrode angle
Undercut — a groove melted into the base metal along the weld toe — results from excessive current, excessively fast travel speed, or improper electrode angle directing heat toward the plate edge rather than the joint.
Written and edited by Nathan Beja, founder of Practice Test Geeks, with AI assistance. Exam facts are checked against the official sources linked below. Editorial policy
Sources & references
Exam facts on this page (fees, format, dates, passing scores) are checked against these official sources; the date is our last check. Editorial policy
- aws.amazon.com — Fees, exam format, time limit, score validity, renewal, passing score, retake fee, retake policy, score release, test delivery · verified Nov 2026