Gas Tungsten Arc Welding (GTAW/TIG) Fundamentals Flashcards
6 cards from real AWS practice questions. Tap to flip, then mark Knew It or Still Learning — missed cards come back until you master them.
Read the first 6 Gas Tungsten Arc Welding (GTAW/TIG) Fundamentals flashcards as text
In GTAW of aluminum with AC, the 'cleaning action' occurs during:
Answer: The electrode-positive (EP) half cycle, when electrons flow from work to electrode
During the electrode-positive half cycle in AC GTAW, electrons flow from the base metal to the electrode, bombarding the oxide layer on the aluminum surface and breaking it up — this is the cathodic cleaning action.
Hot cracking in GTAW austenitic stainless steel welds is prevented primarily by:
Answer: Controlling weld metal composition to include 3–8% ferrite (FN)
Maintaining 3–8% ferrite number (FN) in austenitic stainless weld metal provides ferrite that interrupts the continuous austenite grain boundaries, preventing solidification (hot) cracking.
The interpass temperature limit for GTAW on austenitic stainless steel is critical because:
Answer: Excessive heat input promotes sensitization (carbide precipitation) and reduces corrosion resistance in the HAZ
In austenitic stainless steel, the sensitization range is 800–1500°F. If interpass temperature remains in this range, chromium carbides precipitate at grain boundaries, depleting chromium and causing intergranular corrosion susceptibility.
When performing GTAW on a 6G pipe qualification test, the '6G' position means:
Answer: The pipe is fixed at 45 degrees, not rotated — the welder must weld in all positions in one test
The 6G position fixes the pipe at a 45-degree incline; the pipe is not rotated, so the welder must weld through all positions (overhead, vertical, horizontal, flat) in a single test pass.
Filler metal ER4043 vs. ER5356 for GTAW aluminum welding: which has better crack resistance and why?
Answer: ER4043 — silicon increases weld fluidity and resists solidification cracking
ER4043 (4-5% Si) has better solidification crack resistance because silicon widens the solidification range less and produces a more fluid pool that feeds solidification shrinkage, reducing hot cracking tendency.
AWS D1.2 (Structural Welding Code — Aluminum) differs from D1.1 in that it:
Answer: Specifically addresses aluminum alloy groups, temper conditions, and aluminum-specific NDE requirements
AWS D1.2 is specifically written for structural aluminum welding and addresses aluminum alloy groups (1xxx–7xxx), temper designations (T4, T6, etc.), filler metal selection, and NDE methods appropriate for aluminum's unique properties.
Written and edited by Nathan Beja, founder of Practice Test Geeks, with AI assistance. Exam facts are checked against the official sources linked below. Editorial policy
Sources & references
Exam facts on this page (fees, format, dates, passing scores) are checked against these official sources; the date is our last check. Editorial policy
- aws.amazon.com — Fees, exam format, time limit, score validity, renewal, passing score, retake fee, retake policy, score release, test delivery · verified Nov 2026