  1. The first adhesive dispensed from a new cartridge and mixing nozzle should be handled how?

    Answer: Discarded until the mixture shows a uniform color, as directed by the MPII

    Initial output may be improperly mixed, so it is wasted until the color is uniform.

  2. An inspector sees an installer reuse a mixing nozzle after the adhesive's gel time has passed. What is the concern?

    Answer: Partially cured adhesive in the nozzle can prevent proper mixing and flow

    Once gel time is exceeded, adhesive begins hardening in the nozzle and a new nozzle is required.

  3. Why must the inspector confirm the base material temperature before installation?

    Answer: Gel and cure times, and permissible installation, depend on concrete temperature per the MPII

    MPIIs specify allowable temperature ranges and cure times that vary with base material temperature.

  4. An anchor is disturbed or loaded before the full cure time has elapsed. What should the inspector do?

    Answer: Document the nonconformance and report it to the engineer of record

    Premature loading can compromise bond, so it must be recorded and evaluated by the engineer.

  5. What does a proof load test performed in the field typically verify?

    Answer: That the installed anchor can resist a specified test load without unacceptable displacement or failure

    Proof loading confirms installation adequacy at a specified load, not ultimate capacity.

  6. Which observation during injection indicates a likely void in the hole?

    Answer: The installer fills from the top of the hole instead of from the bottom

    Filling from the top can trap air pockets, while bottom-up injection prevents voids.

  7. Where would an inspector find the qualified conditions of use, such as cracked concrete or seismic suitability, for an adhesive?

    Answer: The product's evaluation report (e.g., ICC-ES ESR) based on ACI 355.4 testing

    Evaluation reports summarize ACI 355.4 qualification results and allowable conditions of use.

Written and edited by , founder of Practice Test Geeks, with AI assistance. Exam facts are checked against the official sources linked below. Editorial policy

Sources & references

Exam facts on this page (fees, format, dates, passing scores) are checked against these official sources; the date is our last check. Editorial policy

  1. concrete.org — Fees, retake fee, test delivery, exam format, passing score, renewal, time limit, score validity, score release, eligibility · verified Nov 2026