ACI Adhesive Anchor Installer Certification Exam — Questions and Answers
Question 1: A wire brush slides into the hole with no resistance. What does this indicate?
- The hole is perfectly clean
- The brush is ideal for the job
- The adhesive can be injected immediately
- The brush is worn or undersized and should be replaced (Correct answer)
Correct answer: The brush is worn or undersized and should be replaced
A brush must contact the hole wall to scrub dust loose; no resistance means it is too small or worn.
Question 2: How should empty adhesive cartridges and partially cured adhesive waste generally be disposed of?
- According to the SDS and local environmental regulations (Correct answer)
- Poured into the nearest storm drain
- Burned on site
- Buried in the excavation backfill
Correct answer: According to the SDS and local environmental regulations
The SDS disposal section and local rules govern chemical waste disposal.
Question 3: Which installation moisture condition may be allowed only if the product's ESR specifically qualifies it?
- Concrete at room temperature
- Holes drilled to full depth
- Dry concrete
- Water-filled holes (Correct answer)
Correct answer: Water-filled holes
Water-filled and submerged holes are allowed only when the product has been qualified for those conditions.
Question 4: The minimum spacing between adhesive anchors is most commonly expressed as a multiple of:
- The anchor rod diameter (d_a)
- The concrete compressive strength (f'c)
- The anchor hole diameter (d_o)
- The effective embedment depth (h_ef) (Correct answer)
Correct answer: The effective embedment depth (h_ef)
Minimum anchor spacing is typically expressed as a multiple of the effective embedment depth (h_ef) to ensure adequate separation of bond stress zones.
Question 5: What does a mismatched ratio of resin to hardener most likely cause?
- Improper or incomplete cure and reduced strength (Correct answer)
- Better hole penetration
- No effect because the nozzle corrects it
- Faster and stronger cure
Correct answer: Improper or incomplete cure and reduced strength
Adhesives are formulated for a specific mix ratio; deviations can prevent full cure.
Question 6: What does a uniform, consistent color of extruded adhesive indicate?
- The adhesive has fully cured
- The hole is clean
- The cartridge is expired
- Proper mixing of the components (Correct answer)
Correct answer: Proper mixing of the components
Many products use contrasting component colors so a uniform blend shows proper mixing.
Question 7: An installer notices the adhesive cartridges are past their expiration date. What is the correct action?
- Use them only for non-structural anchors
- Use them if they still dispense
- Do not use them; get adhesive that is within its shelf life (Correct answer)
- Mix them with fresh adhesive
Correct answer: Do not use them; get adhesive that is within its shelf life
Expired adhesive may not perform as qualified, so it must not be used.
Question 8: How does temperature influence adhesive performance?
- Has no impact
- It controls curing and viscosity (Correct answer)
- Only color is affected
- It determines concrete type
Correct answer: It controls curing and viscosity
Temperature significantly impacts the chemical reaction rate of adhesive curing and the physical property of viscosity. Higher temperatures generally accelerate curing and reduce viscosity, while lower temperatures slow curing and increase viscosity. Understanding and controlling these effects are crucial for proper mixing, installation, and ensuring the adhesive achieves its intended bond strength within the specified timeframes.
Question 9: Before drilling into an existing concrete slab or wall, which hazard check is most important for compliance and safety?
- Locate embedded conduits, post-tensioning tendons, and rebar (Correct answer)
- Check the concrete's original placement temperature
- Confirm the building's occupancy load
- Verify the paint color of the surface
Correct answer: Locate embedded conduits, post-tensioning tendons, and rebar
Striking tendons, live conduits, or rebar can cause injury and structural damage.
Question 10: Mixed adhesive leaving the nozzle shows light and dark streaks. What does this most likely indicate?
- The concrete is too dry
- The hole is too deep
- The adhesive is fully cured
- The two components are not mixing completely (Correct answer)
Correct answer: The two components are not mixing completely
Streaks mean the resin and hardener are not mixed properly, so that adhesive must not go into the hole.
Question 11: An installer notices the ambient and base material temperature is below the MPII's minimum installation temperature. What should be done?
- Heat the adhesive with an open flame
- Install and double the cure time without approval
- Install anyway since temperature only affects appearance
- Do not install until conditions meet MPII limits or follow approved conditioning procedures (Correct answer)
Correct answer: Do not install until conditions meet MPII limits or follow approved conditioning procedures
Installing outside qualified temperature ranges can prevent proper cure and strength.
Question 12: Which best describes the scope of Mechanical Systems & Maintenance in professional practice?
- An outdated concept no longer relevant to modern practice
- A narrow topic relevant only to entry-level professionals
- A comprehensive area covering both theoretical foundations and practical applications (Correct answer)
- A theoretical framework with no practical applications
Correct answer: A comprehensive area covering both theoretical foundations and practical applications
Mechanical Systems & Maintenance encompasses both theoretical foundations and practical applications that are essential to professional practice in this field.
Question 13: What is 'gel time' (working time) for an adhesive anchor product?
- The time until the anchor can be fully loaded
- The time the cartridge can be stored after opening
- The time required to clean the hole
- The time available after mixing to insert and position the anchor element (Correct answer)
Correct answer: The time available after mixing to insert and position the anchor element
Gel time is the window during which the anchor element can still be inserted and adjusted.
Question 14: Partway through a job, adhesive starts to stiffen inside the mixing nozzle. What should the installer do?
- Squeeze harder to force the adhesive through
- Cut the nozzle shorter and continue
- Warm the nozzle with a torch
- Replace the nozzle with a new manufacturer-specified one and discard the first output (Correct answer)
Correct answer: Replace the nozzle with a new manufacturer-specified one and discard the first output
Once gel time is exceeded the nozzle is partly cured, so replace it and discard the initial output until the color is uniform.
Question 15: At approximately what ground-fault current does a typical personnel GFCI trip?
- 50 mA
- About 5 mA (Correct answer)
- 1 A
- 100 mA
Correct answer: About 5 mA
Personnel GFCIs trip at roughly 4–6 mA to prevent dangerous shock.
Question 16: What is the most important competency assessed in Blueprint Reading & Technical Drawings for professionals in this field?
- Applied knowledge and practical problem-solving ability (Correct answer)
- Years of experience without demonstrated skill
- Memorization of textbook definitions only
- Academic credentials without practical application
Correct answer: Applied knowledge and practical problem-solving ability
Blueprint Reading & Technical Drawings assessment focuses on applied knowledge and practical problem-solving ability, ensuring professionals can effectively perform in real-world situations.
Question 17: Which property describes the tendency of an adhesive anchor to gradually displace under long-term sustained tension load?
- Creep (Correct answer)
- Thixotropy
- Exotherm
- Shrinkage
Correct answer: Creep
Creep is time-dependent deformation under sustained load and is a key concern for adhesive anchors.
Question 18: An anchor is disturbed or loaded before the full cure time has elapsed. What should the inspector do?
- Add more adhesive around the top of the hole
- Approve it if the delay was less than one hour
- Document the nonconformance and report it to the engineer of record (Correct answer)
- Ignore it if the anchor still looks straight
Correct answer: Document the nonconformance and report it to the engineer of record
Premature loading can compromise bond, so it must be recorded and evaluated by the engineer.
Question 19: Before using a wire brush to clean a drilled hole, how should the installer check that the brush is still usable?
- Check that the brush diameter is larger than the hole and gives noticeable resistance when inserted (Correct answer)
- Verify the brush has been soaked in solvent
- Make sure the brush handle is at least 12 inches long
- Confirm the brush is the same color as new
Correct answer: Check that the brush diameter is larger than the hole and gives noticeable resistance when inserted
A worn brush that slides in with no resistance won't scrub the hole walls and must be replaced.
Question 20: Who normally checks adhesive expiration dates, hole dimensions, and hole cleaning during inspected adhesive anchor work?
- The ready-mix supplier
- The architect
- The building owner
- The special inspector (Correct answer)
Correct answer: The special inspector
The special inspector verifies the product, its expiration date, hole drilling, cleaning, and installation against the approved documents.
Question 21: Under OSHA's respirable crystalline silica standard for construction (29 CFR 1926.1153), what is the permissible exposure limit (PEL) as an 8-hour TWA?
- 50 µg/m³ (Correct answer)
- 10 µg/m³
- 25 µg/m³
- 100 µg/m³
Correct answer: 50 µg/m³
OSHA set the silica PEL at 50 micrograms per cubic meter of air averaged over an 8-hour day.
Question 22: When drilling into cracked concrete for adhesive anchors, what additional design consideration is required?
- Simply choosing a larger diameter anchor
- Filling the crack with epoxy before drilling
- Use of crack-rated adhesive and reduced characteristic resistance values (Correct answer)
- No special consideration is needed
Correct answer: Use of crack-rated adhesive and reduced characteristic resistance values
Cracked concrete reduces the confinement around the anchor, so ACI 318 requires crack-rated products and appropriately reduced capacity values in design.
Question 23: An inspector sees an installer reuse a mixing nozzle after the adhesive's gel time has passed. What is the concern?
- Partially cured adhesive in the nozzle can prevent proper mixing and flow (Correct answer)
- The nozzle will change the adhesive color permanently
- Reused nozzles increase cure time to several weeks
- There is no concern; nozzles can always be reused
Correct answer: Partially cured adhesive in the nozzle can prevent proper mixing and flow
Once gel time is exceeded, adhesive begins hardening in the nozzle and a new nozzle is required.
Question 24: Which hole-cleaning sequence is commonly specified in MPIIs for hammer-drilled holes?
- Brush once only
- Blow once then inject
- Blow, brush, blow, repeated as the MPII specifies (Correct answer)
- Rinse with water then inject immediately
Correct answer: Blow, brush, blow, repeated as the MPII specifies
Typical MPIIs require alternating compressed air and brushing cycles to remove drilling dust.
Question 25: When starting a new cartridge, why is the first adhesive dispensed thrown away?
- It may not be properly mixed until the color is uniform (Correct answer)
- It is too hot
- It is required for warming the nozzle
- It contains packing air only
Correct answer: It may not be properly mixed until the color is uniform
Discard the initial output until it shows a uniform color, which confirms the components are mixed.
Question 26: Which ANSI standard governs occupational eye and face protection that installers should wear while drilling and cleaning holes?
- ANSI A10.3
- ANSI B11.19
- ANSI Z87.1 (Correct answer)
- ANSI Z359.1
Correct answer: ANSI Z87.1
ANSI/ISEA Z87.1 covers occupational eye and face protection devices.
Question 27: For overhead or deep horizontal holes, which accessory helps fill the hole properly and keeps adhesive from running out?
- Rubber grommet
- Duct tape over the hole
- Piston plug with extension tubing (Correct answer)
- Plastic wall anchor sleeve
Correct answer: Piston plug with extension tubing
A piston plug on extension tubing lets the hole fill from the back while back pressure pushes the nozzle out, limiting air voids and sag.
Question 28: Which situation requires the installer to hold a certification such as ACI/CRSI Adhesive Anchor Installer under ACI 318?
- Installing adhesive anchors horizontally or upwardly inclined to resist sustained tension (Correct answer)
- Installing mechanical expansion anchors only
- Placing concrete slabs on grade
- Installing cast-in-place headed studs
Correct answer: Installing adhesive anchors horizontally or upwardly inclined to resist sustained tension
ACI 318 requires certified installers for adhesive anchors in horizontal or upwardly inclined orientations under sustained tension.
Question 29: An epoxy adhesive contacts an installer's bare skin. What is the recommended first action?
- Let it cure and peel it off
- Cover it with a bandage and continue working
- Wipe it off with acetone or solvent
- Wash the area with soap and water and follow SDS first-aid guidance (Correct answer)
Correct answer: Wash the area with soap and water and follow SDS first-aid guidance
Soap and water removal is standard; solvents can drive resins deeper into the skin.
Question 30: What is a typical function of an air nozzle with an extension when blowing holes?
- To cool the drill bit
- To spray adhesive
- To dry the concrete surface only
- To reach the bottom of the hole and blow out dust (Correct answer)
Correct answer: To reach the bottom of the hole and blow out dust
Air must reach the hole bottom to expel dust from the full depth.
Question 31: What PPE is typically appropriate when drilling and cleaning holes?
- No PPE needed for short holes
- A welding helmet
- Eye protection, hearing protection, and respiratory protection (Correct answer)
- Only gloves
Correct answer: Eye protection, hearing protection, and respiratory protection
Drilling creates noise and silica dust, and cleaning can eject debris.
Question 32: In ACI 355.4, what do the adhesive anchor temperature categories describe?
- The temperature of the drill bit
- Allowable installation and storage temperatures for the cartridge
- Long-term and short-term maximum in-service concrete temperatures the anchor is qualified for (Correct answer)
- Required curing temperatures for the concrete
Correct answer: Long-term and short-term maximum in-service concrete temperatures the anchor is qualified for
Temperature categories set the maximum long-term and short-term base material service temperatures at which the bond values apply.
Question 33: For substrate temperatures below the adhesive manufacturer's minimum installation temperature, what corrective action is acceptable?
- Warm the substrate to the required temperature range before and during installation (Correct answer)
- Switch to a mechanical anchor without changing specifications
- Apply heat only after the adhesive is injected
- Install the anchor and simply wait longer for cure
Correct answer: Warm the substrate to the required temperature range before and during installation
Heating the substrate (with heat blankets, heat guns, etc.) before and during installation ensures the adhesive reaches the minimum temperature required to initiate and sustain the cure reaction.
Question 34: The 'critical edge distance' (c_ac) specified for an adhesive anchor system is determined by:
- The engineer of record on a project-by-project basis using ACI 318 equations
- OSHA field safety inspectors during installation inspections
- Testing and product qualification per ICC-ES AC308 and published in the product evaluation report (Correct answer)
- The local building official based on site-specific conditions
Correct answer: Testing and product qualification per ICC-ES AC308 and published in the product evaluation report
The critical edge distance for a specific adhesive anchor product is established through testing under ICC-ES AC308 protocols and is published in the product's evaluation report (ESR).
Question 35: An anchor is disturbed or loaded before the full cure time listed in the MPII. What is the compliance concern?
- The bond may be compromised and the anchor may not achieve design strength (Correct answer)
- It only affects the anchor's appearance
- It speeds up curing
- It is acceptable if done within 24 hours
Correct answer: The bond may be compromised and the anchor may not achieve design strength
Loading or disturbing anchors before full cure can damage the bond.
Question 36: When an adhesive anchor must be placed closer to an edge than the critical edge distance but farther than the minimum edge distance, the design approach is to:
- Install supplemental adhesive on the anchor rod threads
- Increase the embedment depth proportionally to offset the reduced edge distance
- Use a larger diameter anchor rod to compensate
- Apply a reduction factor to the anchor's tensile and shear capacity (Correct answer)
Correct answer: Apply a reduction factor to the anchor's tensile and shear capacity
When the edge distance falls between the minimum and critical values, ACI 318 requires applying edge distance modification factors that reduce the calculated anchor capacity.
Question 37: Which extension cord gauge can safely carry the most current?
- 10 AWG (Correct answer)
- 16 AWG
- 12 AWG
- 14 AWG
Correct answer: 10 AWG
A lower AWG number means a thicker conductor with higher current capacity.
Question 38: Which IBC chapter sets the special inspection requirements that apply to post-installed anchors?
- Chapter 16
- Chapter 19
- Chapter 10
- Chapter 17 (Correct answer)
Correct answer: Chapter 17
IBC Chapter 17 covers special inspections and tests, including post-installed anchors in concrete.
Question 39: An installer notices that achieving the specified center-to-center spacing is impossible due to existing reinforcement. The correct action is to:
- Increase the embedment depth to compensate for reduced spacing
- Relocate all anchors to the opposite face of the member
- Reduce the anchor diameter to fit between the rebar
- Notify the engineer of record and await revised instructions before drilling (Correct answer)
Correct answer: Notify the engineer of record and await revised instructions before drilling
When specified spacing cannot be achieved due to field conditions, the installer must notify the engineer of record, who must evaluate whether revised anchor placement is acceptable.
Question 40: What is the recommended approach to staying current in Blueprint Reading & Technical Drawings?
- Waiting for regulatory changes to force updates
- Reviewing initial training materials once per year
- Relying solely on past experience
- Regular professional development, industry publications, and peer collaboration (Correct answer)
Correct answer: Regular professional development, industry publications, and peer collaboration
Staying current in Blueprint Reading & Technical Drawings requires ongoing professional development, reading industry publications, and collaborating with peers to share knowledge and best practices.
Question 41: What marking identifies a double-insulated power tool?
- A UL triangle symbol
- A green ground screw
- A square within a square symbol (Correct answer)
- A red power indicator
Correct answer: A square within a square symbol
The square-within-a-square symbol indicates double insulation.
Question 42: A piston plug is used with adhesive injection primarily to help with which installations?
- Mechanical expansion anchors
- Holes in wood framing
- Deep, horizontal, or overhead holes to fill without air voids (Correct answer)
- Shallow vertical-down holes
Correct answer: Deep, horizontal, or overhead holes to fill without air voids
Piston plugs help fill holes from the bottom up and reduce air pockets in deep, horizontal, or overhead holes.
Question 43: What is the main reason the inspector verifies adhesive storage conditions on site?
- Improper storage temperatures can degrade the adhesive before use (Correct answer)
- Storage affects only the label legibility
- Storage determines the drill bit size
- Storage conditions are never specified by manufacturers
Correct answer: Improper storage temperatures can degrade the adhesive before use
MPIIs specify storage temperature ranges to preserve adhesive performance.
Question 44: Adhesive stored in a hot truck cures too fast at the jobsite. What is the root cause?
- Wrong rod grade
- Storage temperature outside the manufacturer's recommended range (Correct answer)
- Too small a hole
- Wrong drill bit
Correct answer: Storage temperature outside the manufacturer's recommended range
The manufacturer specifies a storage temperature range, and adhesive stored outside it may behave abnormally.
Question 45: What tool is used to brush the inside of a drilled hole during the cleaning process?
- A wire gauge probe
- A soft-bristle paintbrush
- A wire brush sized to the hole diameter (Correct answer)
- A cotton swab
Correct answer: A wire brush sized to the hole diameter
A wire brush matched to the hole diameter scrubs loose concrete particles from the borehole walls, which compressed air alone cannot remove.
Question 46: What does a proof load test performed in the field typically verify?
- The expiration date of the adhesive
- The compressive strength of the concrete
- That the installed anchor can resist a specified test load without unacceptable displacement or failure (Correct answer)
- The ultimate failure load of every anchor
Correct answer: That the installed anchor can resist a specified test load without unacceptable displacement or failure
Proof loading confirms installation adequacy at a specified load, not ultimate capacity.
Question 47: Why should a dispenser's piston rod and trigger mechanism be cleaned after use?
- Cleaning lowers the adhesive viscosity
- It increases the adhesive's gel time
- It is required to activate the cartridge
- Cured adhesive buildup can cause uneven dispensing and tool failure (Correct answer)
Correct answer: Cured adhesive buildup can cause uneven dispensing and tool failure
Hardened residue binds moving parts and leads to inconsistent ratio or dispenser jamming.
Question 48: Which document should an inspector use as the primary reference for the correct installation procedure of a specific adhesive product?
- The concrete mix design submittal
- A general concrete construction textbook
- The contractor's daily log
- The Manufacturer's Printed Installation Instructions (MPII) (Correct answer)
Correct answer: The Manufacturer's Printed Installation Instructions (MPII)
The MPII defines the product-specific drilling, cleaning, injection, and cure requirements that must be followed.
Question 49: Who is responsible for approving adhesive anchor installations?
- The adhesive manufacturer.
- A qualified inspector or structural engineer. (Correct answer)
- The project architect.
- The construction crew foreman.
Correct answer: A qualified inspector or structural engineer.
Adhesive anchor installations are critical structural components, and their proper execution directly impacts the safety and integrity of a structure. Therefore, a qualified inspector or structural engineer is responsible for approving these installations. This ensures that the anchors meet design specifications, comply with building codes, and adhere to industry standards for performance and safety.
Question 50: Which PPE is most appropriate when handling two-part epoxy adhesives?
- Leather work gloves only
- Chemical-resistant nitrile gloves and safety glasses (Correct answer)
- No PPE if handled briefly
- Cotton gloves and a dust mask
Correct answer: Chemical-resistant nitrile gloves and safety glasses
Nitrile gloves resist epoxy penetration and eye protection guards against splashes.
Question 51: A detail labels the anchor as installed overhead and resisting sustained tension. What does ACI 318 require for this installation?
- Only a visual inspection after cure
- Installation by a certified adhesive anchor installer (Correct answer)
- No special requirement beyond the MPII
- Use of a mechanical expansion anchor instead
Correct answer: Installation by a certified adhesive anchor installer
ACI 318 requires adhesive anchors installed horizontally or upwardly inclined under sustained tension to be installed by ACI/CRSI-certified personnel.
ACI Adhesive Anchor Installer Certification Exam
This certification program validates the knowledge and skills of individuals installing adhesive anchors in concrete, ensuring proper installation techniques and safety.
Exam Rules
- You can skip questions and return to them later
- Flag questions for review before submitting
- No feedback shown until you submit the entire exam
- Unanswered questions count as wrong — answer everything
- 10 pretest questions are mixed in and don't affect your score
- Timer auto-submits when time runs out
- Your progress is auto-saved every 30 seconds
Practice questions written with AI assistance and published by Nathan Beja, founder of Practice Test Geeks. They are not real exam questions. Exam facts are checked against the official sources linked below. Editorial policy
Sources & references
Exam facts on this page (fees, format, dates, passing scores) are checked against these official sources; the date is our last check. Editorial policy
- concrete.org — Fees, retake fee, test delivery, exam format, passing score, renewal, time limit, score validity, score release, eligibility · verified Nov 2026