What is 'porosity' in a weld and what commonly causes it?
Answer: Gas pockets trapped in the solidifying weld metal, often from contamination or moisture
Porosity results from gases (hydrogen, oxygen, nitrogen) becoming trapped as the weld pool solidifies, commonly caused by moisture, contamination, or inadequate shielding.
Which electrode designation is a low-hydrogen SMAW electrode?
Answer: E7018
E7018 has a low-hydrogen iron powder coating (indicated by the '8' suffix), requiring storage in a rod oven to prevent moisture absorption.
What does 'undercutting' refer to in welding inspection?
Answer: A groove melted into the base metal at the weld toe that is not filled by weld metal
Undercut is a groove or channel burned into the base metal along the weld toes or root that weakens the joint by reducing cross-sectional area.
In plasma arc welding (PAW), what distinguishes the 'keyhole' technique from conventional welding?
Answer: A focused plasma jet penetrates completely through the base metal, creating a hole that is filled as the torch progresses
The keyhole technique in PAW uses a constricted, high-energy plasma column to pierce through the workpiece; the molten metal flows around and behind, producing full-penetration welds in one pass.
What is the significance of the 'interpass temperature' in multi-pass welding?
Answer: It is the maximum temperature of the weld area between passes, controlled to prevent metallurgical damage
Interpass temperature is the maximum allowed temperature of the weld zone before depositing the next pass, preventing excessive heat input that can degrade toughness and mechanical properties.
Which welding position is designated as '5G' in the AWS classification system?
Answer: Pipe welded with its axis horizontal and fixed (not rotated)
5G designates pipe with its axis horizontal and the pipe fixed in place, requiring the welder to weld in all positions (flat, vertical, and overhead) around the pipe.
What is 'cold lap' (overlap) in welding?
Answer: Weld metal that extends beyond the weld toe and lies on the base metal without fusion