Moisture Mitigation Systems Flashcards
7 cards from real CFI practice questions. Tap to flip, then mark Knew It or Still Learning — missed cards come back until you master them.
Read the first 7 Moisture Mitigation Systems flashcards as text
Which scenario would cause a calcium chloride (ASTM F1869) test to give a falsely LOW moisture reading?
Answer: Testing on a very cold slab with low ambient temperature
Cold slab temperatures slow vapor emission, resulting in lower calcium chloride weight gain and an artificially low MVER reading that does not reflect real service conditions.
What does 'alkalinity' of a concrete slab have to do with moisture mitigation?
Answer: High alkalinity caused by moisture can destroy adhesive bonds and cause pH-sensitive flooring to fail
Moisture moving through concrete carries alkaline salts to the surface; this high pH environment can break down adhesives and degrade pH-sensitive flooring products.
Which flooring installation method is considered the most moisture-tolerant for use over problematic concrete slabs?
Answer: Floating installation with a foam underlayment
Floating floor installations do not bond directly to the slab, allowing some moisture tolerance, though a vapor retarder is still typically required beneath them.
When a moisture mitigation membrane is required to span cracks in a concrete slab, what additional step is typically needed?
Answer: Fill or reinforce cracks with a flexible crack-isolation material before applying the membrane
Active or moving cracks must be filled with a flexible polyurethane or epoxy filler and may require crack-isolation fabric bridging before the membrane to prevent future cracking through the coating.
What does the abbreviation 'CSP' stand for in the context of concrete surface preparation for coatings?
Answer: Concrete Surface Profile
CSP stands for Concrete Surface Profile, a scale from 1–9 defined by ICRI that describes the texture and roughness of prepared concrete surfaces.
A moisture mitigation system warranty is typically voided if which condition exists at the time of installation?
Answer: Slab RH exceeds the product's rated maximum at the time of application
Applying a moisture mitigation product when slab RH or MVER exceeds the product's specified maximum rated threshold voids the product warranty as the coating is not designed for that extreme.
What is the purpose of conducting a 'bond test' (pull test) after applying a moisture mitigation membrane?
Answer: To verify that the mitigation membrane has adequately bonded to the concrete substrate