โ† All C33 Flashcard Decks

Identifying and Remedying Paint Failures and Defects Flashcards

7 cards from real C33 practice questions. Tap to flip, then mark Knew It or Still Learning โ€” missed cards come back until you master them.

Read the first 7 Identifying and Remedying Paint Failures and Defects flashcards as text
  1. A painted wood surface shows a condition where the paint film has split along the wood grain lines. What is this defect called?

    Answer: Checking

    Checking is the splitting of the paint film along or across wood grain, typically caused by overly thick paint or inadequate flexibility of the coating.

  2. Which condition describes a paint failure where new paint peels away from the previous coat but both remain bonded to the substrate?

    Answer: Intercoat adhesion failure

    Intercoat adhesion failure occurs when insufficient surface preparation, incompatible products, or insufficient dry time causes the new coat to separate from the previous coat.

  3. A homeowner notices a dark, fuzzy growth appearing through a freshly painted bathroom wall. What is the most likely cause?

    Answer: Mold or mildew growth from moisture not fully remediated before painting

    Painting over active or inadequately treated mold without proper remediation allows growth to continue and penetrate through the new paint film.

  4. When painting over a glossy surface without sanding or etching, which failure mode is most likely to occur?

    Answer: Poor adhesion leading to peeling

    Glossy surfaces offer insufficient mechanical or chemical bonding sites, so the new coat fails to adhere and eventually peels.

  5. What paint defect results from applying a solvent-based topcoat over a water-based primer that has not fully cured?

    Answer: Lifting or wrinkling of the topcoat

    The solvents in the topcoat soften the uncured primer beneath, causing the topcoat to wrinkle or lift as trapped solvents escape.

  6. A painter observes that a recently applied exterior coat has a dull, hazy appearance in certain areas compared to the rest of the wall. This is called:

    Answer: Flashing

    Flashing is an uneven sheen caused by differences in porosity, application technique, or touch-up painting over a dried coat without feathering properly.

  7. Which of the following is the correct remediation sequence for a surface exhibiting heavy alligatoring?

    Answer: Remove all failing paint, treat the substrate, prime, and repaint

    Alligatoring indicates a fundamentally failed paint system; complete removal to bare substrate, proper prep, priming, and repainting is the only reliable long-term fix.