A weld with excessive convexity (high crown) is problematic because:
-
A
It wastes filler metal but has no structural consequence
-
B
It creates stress concentration at the weld toes and may indicate improper deposition technique
-
C
It makes slag removal more difficult
-
D
It indicates insufficient penetration